Thoughtful fabric guidance for a more comfortable homeExplore the journal
Search

Fabric Shrinkage Calculator

Fabric testing tool

See exactly how your fabric changed.

Measure dimensional change after washing or treatment across length, width, and total area. Mark and measure the same test area before and after treatment, with the fabric relaxed and measured in the same way.

05

Enter before and after sizes

Length is required. Width adds crosswise and total area shrinkage.

Measurement unit
Before treatmentAfter treatment
cm
cm
cm
cm
Testing tip

Precondition the sample, mark a sufficiently large square, follow the intended wash and drying method, then let it relax before remeasuring.

Results describe the tested sample and treatment only. Fibre content, construction, finishing, wash temperature, agitation, and drying method can all change shrinkage behavior.

How to use the Fabric Shrinkage Calculator

How to measure

  1. Cut a test piece at least 50 × 50 cm (or 20 × 20 in) and mark a measured square on it with a fabric pen.
  2. Measure the marked length and width before washing.
  3. Wash and dry it exactly the way the finished item will be washed and dried.
  4. Lay it flat without stretching, measure the marks again and enter both sets of measurements.

The formula

  • Shrinkage % = (before − after) ÷ before × 100
  • Area change % = (1 − (after length × after width) ÷ (before length × before width)) × 100

A negative result means the fabric grew rather than shrank. Result bands: under 2% minimal, 2–5% moderate, over 5% high.

Worked example

A test square measured 100 × 50 cm before washing and 95 × 49 cm after.

Length shrinkage = (100 − 95) ÷ 100 = 5% (moderate). Width shrinkage = (50 − 49) ÷ 50 = 2%. Area shrinkage = 1 − (95 × 49) ÷ (100 × 50) = 6.9%.

To end with 100 cm after washing, you would cut about 100 ÷ 0.95 = 105.3 cm.

Common mistakes to avoid

  • Testing a small scrap. Small pieces give unreliable results; use a large test square.
  • Measuring while the fabric is still damp or stretched.
  • Testing with a gentler wash than the item will really get.
  • Assuming shrinkage is the same in both directions — length (warp) often shrinks more than width.

Frequently asked questions

How much does cotton shrink?

Untreated cotton commonly shrinks 3–5%, and sometimes more in a hot wash and tumble dry. Pre-shrunk cotton usually shrinks less than 2%.

How do I calculate fabric shrinkage percentage?

Subtract the after-wash measurement from the before-wash measurement, divide by the before-wash measurement and multiply by 100.

Should I pre-wash fabric before sewing?

Yes for washable fabrics such as cotton and linen, especially for curtains and garments. Pre-washing removes most shrinkage before you cut.

What is acceptable shrinkage?

Under 2% is usually considered minimal. 2–5% is common for natural fibres. Above 5% should be pre-shrunk or allowed for when cutting.

Further reading from the journal